By blind - 1/25/2018 6:59:05 PM
Hi all, I'm new to working with carbon, normally just fiberglass. I've made a bit of a mess trying to make a CF part in polyester gelcoat and fiberglass mould as resin would stick like mad. If I use epoxy gelcoat for mould, can I use fiberglass on the back? I've read that only certain type of fiberglass works with epoxy. What is best to use if normal fiberglass doesn't work?
|
By Hanaldo - 1/26/2018 2:45:46 AM
You can use woven fibreglass or powder bound chop strand mat, it's only regular chop strand mat that doesn't work with epoxy.
|
|