By SHaas - 1/21/2018 8:34:35 AM
Hi there,
how do you manage that the carbon fibre shows every detail of the mould? Using the adhesive spray is problematic because of the irritations on the part, but is there another way. My mould has some cornes and edges and I do not get the fibre sticking so that after the resin infusion there are some bridges and the part is ruined.
Thanks for your ideas!
|
By Warren (Staff) - 1/22/2018 9:21:08 AM
Mostly it is about lay up and bagging technique. If you have enough material to avoid bridging, then in most cases with gradual and careful bagging you should be able to get the fabric into the corners of the mould.
|
|