Hi guys! I've made the mould for my second piece of the project and its surface came out with a lot of imperfections.
I have sanded it but I took off some black gel coat in some parts, so now the polyester resin from the mould is showing up in some spots and the surface isn't decently even yet. I knew the plug wasn't perfect but the mould came out worse than expected.
Here are my questions:
1) can I continue to sand until I get a decently even surface, even though the yellow resin is visible?
2) do I need to re apply the gel coat and then sand it again?
3) I need to to even out the surface with bodywork filler and then apply the gel coat again?
I do not want to make the mould again, so which is the best way to do it in your opinion?