By scottracing - 1/1/2018 3:58:04 PM
I'm trying to find a suitable resin system or clear gel coat that is safe for food use with a decent temperature allowance.
Is there such a material? I've been doing a bit of searching and found the ART resin from the USA which is seemingly ok for food use. But im looking for something that i can possibly use in infusion or snap cure compression moulding.
Any help or direction greatly appreciated.
Cheers Garry
|
By scottracing - 1/7/2018 9:27:57 AM
Thanks for the reply matt, I will certainly make up some tooling for the plates and bowls and then at least It gives me the choice of making them out of preg or doing a infusion.
I think I will make a few test coupons to see what works best, but Im thinking prepreg will be my first option and I can look into clear coats in the future. It will be interesting to see how well it reacts against cutlery scraping against it.