I have five panels for sale with Aerospace grade material these panels are all autoclave cured ranging from 2mm to 15mm in wall thickness. Panels are listed at roughly 1/5th of the manufacturing cost. Please see below.
Image 1 shows a resin infused panel with woven carbon 914 ply measuring 500 x 500 x 2mm this panel shows a little surface porosity, otherwise in excellent condition.
Image 2 shows a uni-directional laminate measuring 540 x 180 x 5mm with excellent surface finish 914 material.
Image 3 shows glossy top CFRP laminate measuring 470 x 470 x 15mm. this panel as a excellent surface finish with hexcel 8552 carbon material.
Bottom Image is a listing for 2 exact items these are uni-directional carbon laminates measuring 1m x 750 x 5mm with 914 grade material
laminate 1 £60.00
laminate 2 £70.00
laminate 3 £100.00
laminates 4 £250 each.