By RyanParle - 12/12/2017 8:12:22 PM
I have just purchased a small cnc router which I plan to use (amongst other things) to make some of my future patterns, the router has a working area of 275mm X 385mm 60mm which will be fine for some of my smaller projects, but for larger projects I was thinking of building the patterns in sections with indexing lugs and bonding the sections together before sanding and sealing. Is this a suitable method? If so what would be a suitable adhesive to use? Ill be using EB700 High Temperature Epoxy Tooling Board.
Many thanks Ryan
|
By RyanParle - 12/13/2017 10:56:09 AM
Thanks Warren, that answers my question nicely.
|
|