By GreyArea - 12/10/2017 1:03:05 PM
I’ve cut a design into carbon fibre that I’m reinstating with clear polyester. The design is quite intricate and fine...think of it as a shallow channel about 1x2mm cross section in places, but about a meter long with branches off it etc.
To exclude Air I’m filling it from the bottom of the design with a syringe. I’ve got a silicone mould on top of it, but I’m getting a lot of seepage at the interface so a lot of excess resin that I then have to remove.
What’s the best way to seal the carbon fibre/silicone interface so that this does not happen?
|
By Warren (Staff) - 12/11/2017 12:35:55 PM
Just use some meths to thin it slightly.
Cleaning brushes and resin is a job for acetone.
|
|