By Rui Roseno - 12/5/2017 11:12:24 PM
Hello, first of all thank you for this forum I hope I can find my answer here  I have a bicycle seat post made of carbon with a head of aluminium (photo on attach). I will cut the carbon on the top to lower it size and need to re-glue the aluminium part to the seatpost. I was thinking on buying the Permabond ET500 but on the description I have noticed that they also recommend the VuduGlu VM100 that don't really need so much preparation and possible a better bond. Wich one do you recommend, or other one?
The idea is to keep it 100% safe because I will ride on top of it and it should not fail under any way of stress!! Thank you!
. 
|
By scottracing - 12/8/2017 1:02:08 PM
as hanaldo says preparation is key here, make sure everything is abraded properly and cleaned with acetone properly.
|
|