By vermachina - 12/1/2017 3:26:06 AM
Dear friend, I am new in this so I am looking for the details of how to make composite sheets for laptop cover Which carbon Fiber need to use How many layers of carbon fibers need use and directions of it? Which chemical resin need to use for it What is the size of vacuum pump I need to use How many peel Ply need use and how Which kind of carbon fiber weaving will be good that outer look will be nice Any specific process
|
By Warren (Staff) - 12/1/2017 9:23:33 AM
Hi Rakesh,