By andy47 - 11/23/2017 12:19:20 PM
I have the Easy Composites resin infusion starter kit with the VP425 vacuum pump. My vacuum gauge is reading min. -27 even if the hose is clamped. In the video tutorial, it was reading -27 and he said “it should be reading -30... well, nowhere near... there's clearly a leak”. I know there is no leak because it stays -27 for hours.

To narrow down issues, I bought a new vacuum gauge and this one reads -29.

Do you have any such experience? Do you think the vacuum pump is working properly?
|
By oekmont - 11/23/2017 5:21:03 PM
Rotary vane pumps are very low maintenance and nearly indestructible. It is very unlikely, that the problem is caused by the pump itself. I would recommend to check the connector, and keep on carbonating.
|
|