By Richardsmith1 - 11/15/2017 10:01:51 PM
Hello, 1st post.
I'm trying to make a pattern as per the airbox video. The pattern coat primer went ok but the gloss coat leaves deep brush marks where I start and end brushing. I can see if I had a simple flat shape I could make full length strokes that this wouldn't be a problem. But this is fairly complex and requires brush strokes from the centre out.
So are there any tips other than spraying to get a smoother gloss coat finish.
Cheers Richard
|
By Warren (Staff) - 11/16/2017 9:16:12 AM
Try and carry the brush straight off the edge of the pattern rather than lifting it if possible. You could use a flat edged piece of plastic to skim over the Hi-Gloss to smooth out any strokes.
|
|