By Junior - 11/11/2017 7:25:19 PM
I'm working on my first project, a carbon fibre kayak seat. I have just laid down my final layer but it came out dry and doesn't have that glossy appearance.
I intend to apply a flowcoat to finish it off but not sure whether I can apply the flowcoat now to rectify the glossy appearance, or should I apply more resin to get it right first? Are there any downsides to putting the flowcoat on now?
|
By Junior - 11/14/2017 3:47:34 PM
Very true. It will have some showing but as my first project I wanted to show off the carbon!
Will see how I get on without.
|
|