By Steve Broad - 11/4/2017 7:10:33 PM
First test of the new DIY 1800mm x 1800mm x 900mm oven was curing the carbon/aramid hockey stick Alex and I made for his girlfriend's birthday. First attempt to gauge weight distribution and strength. Had a few issues which we repaired so it won't stand up to heavy usage but is a good starting point from which we can get data. Used fibreglass to make the mould and this was a mistake as it can only be heated to 93 deg C. This works but takes 12 hours to cure! Next mould will be made properly which will also allow me to run 3BAR pressure inside the stick, thereby enhancing the strength.
|
By Tony2125 - 12/28/2017 9:25:40 PM
Hello Where did you find your polythene tube ? I assume there are different qualities. I also need this for bladder molding Thanks
|
|