I have not used this stuff, It's probably just a flow medium and perforated release film bonded together to make the process a bit easier for large jobs like wind blades, boat hulls etc.
It's likely not so conformable as using separate layers of perf and flow medium so if your parts are small or detailed then this is probably not so good to use.
|