How can i remove Chemical Release Agent?
http://www.talkcomposites.com/Topic24051.aspx
By Jaspen
-
10/15/2017 4:20:03 PM
Hello all
Is there any good way to remove the Chemical Release Agent competely?
Is sand blasting is the way to do it?
Regards
By MarkMK
-
10/16/2017 11:50:53 AM
Or the mould cleaner as sold by EC