 First of all, sorry for the poor English that I have.  I done the vacuum infusion for 10 years.  But I find that it was really difficult to make a perfect carbon parts by Resin Infusion. The reason is when leakage happened in fusion. Those bubbles were in between the layer of Carbon Fabric and Gel Coat which is not happy to see this.  Bascially it was unable to handle.  So I tried no Gel Coat for vacuum infusion. But how to fix the pin holes issue by post processing? Can I use XCR resin to spray after forming? I tried IN2 already. Its viscosity too low
Thanks all advise
By Warren (Staff) - 10/13/2017 8:10:53 AM

No, not at all.  Find out why you are getting pinholes and you will probably be able to get good cosmetic results with no gel coat at all.