By Dezer - 10/2/2017 12:37:08 AM
Hello guys,
I'm having trouble de-moulding one of my molds. Mould made with polyester and the piece was infused with epoxy resin.
What is the best solution to reuse this mould and continue infusing with epoxy resin?
PVA is a good solution? works well with the infusion process?
|
By Dezer - 10/2/2017 11:57:52 AM
For some months I have done this mold. I believe that for this reason will not have any problems with styrene.
I am currently using a hydrocarbon-based chemical mold release and yet one of my infused parts got stuck in the mold.
I will do the infusion test using PVA mold release.
|
|