By Phil_123 - 9/26/2017 1:52:48 PM
Hi I am new to this and could do with some advice.
I am just finishing my MDF plug, I have coated multiple times in pattern coat primer and sanded to P600 all over and really happy with the shape. The problem I have and keep having is that I break through to expose the MDF or filler in really small areas.
I am going to spray on the Pattern Coat Hi Gloss Finish so would this be ok to cover these small areas before making my mould or should I start again with the primer?
I have read other topics about this and i do know that you cannot seal an entire MDF plug with the high gloss but I wandered if I would get away with small area. I was going to Spray the High Gloss then finish with P1200- 1500 then polish.
Thanks in advance
|
By Phil_123 - 9/26/2017 4:54:03 PM
I should have used Pigment. I will do next time.
Ill give it a go and see how it finished over the MDF.
Thanks Warren
|
|