By rmaddock - 9/24/2017 6:22:13 PM
I'm using strips of machined High Density Polyurethane Foam as the core for gunwales in my canoes. Unfortunately, the canoes are 16' long so I need to join some lengths. What would a suitable adhesive be?
|
By Rich (Staff) - 9/25/2017 12:49:25 PM
Alternatively a single part foaming polyurethane such as (Original) Gorilla Glue will work.
|
|