By Interloper393 - 9/20/2017 12:21:07 PM
Hi guys I'm needing some really good cutting bits for the dremel, I mainly skin interior pieces so need to be sharp, last and no too big to cut out small sections after a few resin coats. Cheers
|
By DANNYHOCKIN - 9/22/2017 8:53:48 PM
You mean your topcoat is lifting off as you cut? I've never had any trouble like that before. High speed and I kind of imagine I'm taking material away slowly, rather than cutting a line. Also, I really only us the one that is tapered. I had problems keeping straight cuts with all of the others.
|
|