By Saff - 9/8/2017 9:00:14 PM
Hi guys, as I promised in my presentation topic, here you can see some of my recent the work:
- Mirror cover for Alfa Romeo Giulietta. This is my car, so I can use this to test materials and techniques - Ducati multistrada tank cover and rear wheel fender: some works for a friend of mine. The construction of the mold for the tank cover was quite tricky - engine cover for a focus RS: high temperature resin infusion and oven curing. This was a test for temperature resistance of the resin and the 3d printed spacers: after 1 year of track days he has no problems - backrest for wheelchair: he needed something to support the back, which was durable but also flexible, so I made this carbon sheet. The black plastic supports are 3d printed.
that's all for now 
|
By Kieren1234 - 10/19/2018 1:16:40 PM
I’ve only JUST started carbon skinning but god do I wish I was as good as this!! I guess it’s just something that you get better at the more you do??
|
|