By legenddarcy - 7/25/2017 2:43:58 PM
Hi All Looking for advise on a repair i done. Its a new part from a car bumper spliter owner hit a ramp and smashed the top coat, Now its from a show car for a company so they wanted a quick fix till the new part arrived. I managed to save it for the most part but im getting a darker finish in the repaired area. The parts is made with polyester resin so i used polyester resin to repair and advise? Part is still not finished or polished but when wet sanding you can notice it in its gloss state. any ideas on how to hide or blend the color?

|
|