By Granite - 7/17/2017 1:01:21 PM
Hi,
I baught some SuperSap CLV Clear Epoxy Bio Resin at the start of June, and have used it a few times, and been quite pleased with the results. However when I went to mix up a batch over the weekend the resin part seemed to have turned lumpy, and the viscocity seemed higher than previously.
It looked a bit like it had crystalised partially. I mixed up a batch and it seemed to cure OK but is slightly cloudy. The container has been kept in an unheated garage in the UK but at this time of year I would be supprised if the temperature had been below 12C. Other epoxy I have used has been fine with this kind of storage, even through the winter.
Do you have experiance of the SuperSap beng more suceptable to storage issues than others?
|
By Matt (Staff) - 7/19/2017 2:07:39 PM
Great; thanks for letting us know. I'm glad that sorted the problem - we have known other resins to crystallise rather mysteriously, sometimes during transport through cold courier depots!
|
|