By Interloper393 - 7/4/2017 10:54:26 PM
Hi guys iv been adding the black pigment paste to my resin for the Base coat but it always fish eyes and don't cover the parts very well and leaves bits of non black showing through, any ideas why?
Cheers
|
By Interloper393 - 7/5/2017 12:17:53 AM
80 grit, washing and degreser
|
|