I'm not totally sure the OP isn't after a clear finish over the carbon... Could have used a clear gelcoat, and now wants to clear over the top of that.
Either way, technique is the same really. Needs to be sanded and cleaned. Primer isn't totally necessary, but not a bad idea if trying to colour match.