Talk Composites - The Forum for Advanced Composites
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
Hotcoat?
http://www.talkcomposites.com/Topic23454.aspx
By ian.kelly@basegroup.co.uk
-
6/3/2017 8:35:22 PM
Hi
I've been trying to get into home build surfboards and have seen the term "hotcoat" used regularly for the final outer coat of the board that can be brought up to a high polish. What sort of resin is this. I had a quick search around the net and this site but don't really see anything on this.
I also am doing repairs on a few old boards. Would this "hotcoat" be what you would recommend to use?
Thanks
Ian
By Rich (Staff)
-
6/5/2017 1:29:45 PM
Hi Ian,
The XCR Epoxy Coating Resin works perfectly for hot-coating surfboards; it has the added benefit of being highly UV stable and extremely polishable.