By FLD - 5/21/2017 10:27:10 AM

Ive been making some car seats recently. Look ok but there's a line down the back where the resin spiral tube was.  I infused out from the centre to braid around the outside.  The indentation is not really unexpected but I thought I'd ask people's opinion of these stand-off sleeves for the spiral. Any good? Is there another way?

Thanks

Seat looks like this straight from the mould. Quite pleased with it!
By FLD - 5/22/2017 10:09:50 AM

Thanks warren.