By winty - 4/27/2017 6:47:44 PM
I've miss calculated the amount of resin needed for my mould and haven't achieved 4 layers, is there still an option of applying more within a time frame? or is it best to wait and key in and add more??
|
By Dravis - 4/28/2017 9:39:48 AM
You do not need much time at 60 deg .. The unimoulds I have made were probably at 60 degrees for less than an hour ..
|
|