By baja_patient - 7/19/2012 2:25:04 PM
Hi guys, have bin playing round with my infusions for a while now, tried the spray tack method and as expected it had a negative impact of surface finish. I wasnt too worried as I plan to clear coat the parts anyway.
Nevertheless I plan to try the gelcoat method. What are my advantages of using the GC50 epoxy compatible polyester gelcoat apart from it being cheaper than epoxy gelcoat? UV stability I understand, polishable etc...
Is it worth using a gelcoat if i plan to clear coat the part?
If I try, I am not really looking forward to spraying it in. Can a nice surface be achieved by just brushing the gel on? Or will the brush marks be visible in the surface, in which case it kind of defeats the purpose.
Cheers
|
By baja_patient - 7/20/2012 7:11:46 PM
Thanks guys! Joe that is what I thought, would be too difficult to get an even coat, non blurry etc..
And Matt, that is EXACTLY what I have been waiting for, good on ya, It sounds highly promising and I will be placing an order shortly.