By Dennisw - 11/14/2016 7:10:21 PM
I have started turning pens and now intend to make my own blanks. I am going to use your "water Clear" polyurethane casting resin and our polyurethane pigments to relate the solid colours. Will I be able to use other types of pigment powders, such as "Pearlex" to make contrasting features without extracting from the resins strength? Also, what depth of resin can be put into a mould in one pour? I want to make my blanks about 20mm square.
|
By Warren (Staff) - 12/5/2017 10:18:24 AM
Yes pearlex and other pigment powders should be fine. The water clear PU is limited to 15mm per layer so 20mm would need 2 pours to avoid any exotherming.
|
|