Talk Composites - The Forum for Advanced Composites

Adhesive question

http://www.talkcomposites.com/Topic22118.aspx

By David_Wallis - 10/14/2016 2:11:14 PM

What adhesives would people recommend bonding Composite car body panels to the original body panels?




Had good results previously with windscreen adhesive of all things, much better than sikaflex.




So,




Carbon to Metal (steel)

Glass fibre to Metal (steel)




Thanks
By Fasta - 11/10/2016 2:04:54 PM

Polyurethane adhesive as you have done