I have a repair to do to my waggon following the MOT man trying to close the bonnet with the prop up (crrraaaack!).
It's a CSM laminate so nothing posh.  I've repaired with polyester before but I seem to remember reading that vinylester has a better bond for repairs?  Have I imagined this or is there some truth in it?  I've never used Vinylester before so if it's true are there any pitfalls I should look out for?

Thanks guys
By FLD - 8/22/2016 9:18:17 PM

Thanks guys, I'll fix with some woven glass I have so no worry about binders.  Smile