By Marco Balzano - 7/8/2012 9:40:14 AM
Dear Matt,
I would like to know if the IN2 infusion epoxy resin is sold in red colour or if it is possible to add a red pigment to it.
Regards
Marco
|
By Matt (Staff) - 7/9/2012 8:37:49 AM
Hi Marco,
We don't sell it in red but it would be possible to add a pigment dispersion into the resin. Make sure you use epoxy pigment (not polyester or polyurethane) otherwise you will impair the performance of the resin but providing you use the right pigment, there is not reason why you can pigment any epoxy resin, including our IN2.
--Matt
|
|