By +cosworth - 1/23/2012 10:34:50 PM
I have a problem with pva mold release agent, put the pva with a clean lint-free cloth but when dried pva is not uniform ! out spots where there is thepva? This may not clean the mold? |
By mhdghoul - 2/3/2012 6:27:48 AM
man you have to try everything to see what fits you better , i faced all the above problems and guess what worked with me , a normal brush and sometimes i do 2 layers of pva , after the first is cured , i tried the water adding it didn't work with my pva , i saw many guys using there spray guns to add pva i did and it didn't work with mine until i added alcohol , as for all the above i think everyone was right about solving there problems way .
as for paul trick i think i need to try it too , seems nice and paul is a high expert man
|
|