Hi,
I´ve made a part by RTM and i´ve got a few problems.
The part is composed by:
-one layer of 2x2 twill carbon fiber 200grs
-one layer of soric 2mm
-one layer of 2x2 twill carbon fiber 200grs
Theproblems that occured are:
-the hexagonal shape of the soric has been printed at the first carbon layer
-this same layer has been a little bit dry, and printed the fibre shape at themould.
Here are few fotos attached for you to take a better look:
http://i675.photobucket.com/albums/vv112/pedcrist/Carbon/Firstlayer_1.jpg
http://i675.photobucket.com/albums/vv112/pedcrist/Carbon/Mould_3.jpg
By pedcrist
-
7/8/2012 9:55:13 PM
Thanks for the explanations, Kev!!!
Pedro