I've been offered the use of a split mould to make a clamshell for my car. Seems rude not to! However, its a large split mould with no sealing channels in the flange. It got me thinking....... Can I seal over the split line with a compatible gel coat prior to infusion or is the gel coat stripe likely to let air by?
I'd be grateful for any other suggestions too.