By ECV3 - 5/7/2016 11:39:42 PM

If the final Cure Temp of 80C in a cycle takes 5 hours how long will a final Cure Temp of 85C take ?.

Cheers!
By racecomp - 7/6/2016 1:53:41 AM

Take an hour to ramp up to 55/60 deg C and then hold for an hour, after that start 5 deg C every 20 mins.