By unijacko67 - 4/10/2016 1:23:46 AM

Hi all, I've been asked if I can help a pal out by making a replica heat shield for his Ford Cosworth. It's had foil stuck to the face nearest to the turbo/exhaust and looks like the fine fiberglass cloth on the outside. The outside is black and not resin rich, but I'm really not sure what it has been made of or even if the black is a dust coat of spray, any info would be great.

I'll try to post some pictures, but it's hard to tell from a picture what it could have been made from so any hints and advice as to what could have been used will be a great help, thanks.
By unijacko67 - 4/17/2016 10:56:32 AM

Hope the pictures help, if you can indeed see them as strangely they had got removed or something, cheers.