So I've polished my mould up and have noticed some what look like air line cracks in the gel coat, never had this before is this now going to cause a problem when making the part?

This part was barley rubbed down as it's not a visible bit
http://www.talkcomposites.com/Uploads/Images/e4998654-b193-41e1-88d2-0a13.jpg