which adhesive

http://www.talkcomposites.com/Topic20739.aspx

By 111mattin111 - 3/5/2016 8:12:21 PM

Which adhesive is the best for bonding carbon to carbon, inner and outer skin of carbon car doors,  also when bonding the two together when the adhesive seeps out between the two won't this be visible once it's had its final trim?

Paul
By scottracing - 3/6/2016 10:11:00 PM

I've not used any of the adhesives from ec. I usually use 3m dp490 which is an epoxy 2 part structural adhesive. You can mix micro balloons into the mix to ensure the bond thickness is maintained.