By D3O Phil - 2/8/2016 1:37:09 PM
Hi just starting out on this composites road. mostly with Resin infusion and a few Pre pregs So I'am sure to be asking some odd questions in the future
I attended one of the easy composite training courses a year or so ago so it's nice to get back into the swing of things again
Very happy when my first panel came out firstly flat and secondly looking good.
Phil
|
By D3O Phil - 2/12/2016 5:29:48 PM
It's a company project so I can't say too much.... however
mostly I will be making resin infusion flat panels so I can chop them up for impact and flexural testing, we have various test rigs in house.
would be interested to hear from anyone who also physically tests their samples.
|
|