By fgayford - 2/3/2016 11:13:58 PM

In a youtube clip about carbon fiber guitar production (Composite Acoustics factory tour) They were talking about applying an adhesion promotor before the clear coat. Have any of you knowledge to share on this topic?
Thanks
Fred
PS this is an excellent factory tour I highly recommend you guys watch it.
By fgayford - 2/5/2016 1:24:38 PM

Thanks.

If you type in these into youtube you will get the videos I was talking about. I found them fascinating.




The Making of a CA Guitar Part 1/2




Composite Acoustics Tour, Part I

there is also part 2 and 3