By TomDesign - 1/31/2016 7:13:22 AM

https://www.youtube.com/watch?v=Vwh_SYZLHKs


and any idea where to get? they tell you heat with gun and you lay it easy on top.
By TomDesign - 2/1/2016 11:08:04 AM

they say they can overlay on oem part with heat gun and lay 1 layer resin clear coat and you perfect. how is that is pre pregs need big heat and plastic gonna deformate or melt. and never saw that pre pregs can overlay with resin layer and sand.