Iam making a air cleaner lid like this.
Usualy I use the GC50 gelcoat on my parts, should I skip the gel coat on a engine part because of the heat?
Can I use regular infusion epoxy or should I use hi temp epoxy?
By morepower
-
2/23/2016 9:04:53 PM
A carbon air cleaner lid should be OK.... I do these...