Talk Composites - The Forum for Advanced Composites

What do I use to cut carbon fiber?

http://www.talkcomposites.com/Topic20349.aspx

By deceased10 - 1/25/2016 6:53:27 PM

Hello, I am working on a project and got to trim some edges. I am just wondering what bit I would use on my DREMEL? I know easycomposites sells a tungsten carbide disk meant for cutting carbon fiber, however, I am from Canada and the shipping rate for such a small item seems very high. Does anyone know any alternative bit I could use that I could get at a local Canadian store? 
By Dravis - 1/26/2016 1:27:23 PM

The small diamond cutting wheels that are available for Dremels, cut the thin CF stuff very well .. and they never wear down .. The EC permagrit is better, it does not generate as much heat .