heya, looks like a 300zx nose panel!
how are you getting on with carboning the Z? ive seen youve been tackling the boot, doors and fenders
I made the nose panel in a single piece mould.. you can tell the factory one was made in a single piece, its usually the easiest way to tell if it will release or not.. Nissan already took the guesswork out for you
you have any more pics of the car?