By 67redrocket - 1/6/2016 6:02:04 PM

How do you clean away the wax from your moulds? 

Any good tips? 
By davro - 1/11/2016 2:43:10 AM

I normally scrape the main body of wax with a strong piece of plastic and place used wax into my wax recycling bag.