Hi to everyone, first post.

http://www.talkcomposites.com/Topic20125.aspx

By Spitfire - 1/2/2016 8:11:09 AM

Hello, new member here with my first post on the forum.

I am currently in the carbon fibre laminating business, the company I work for mainly manufactures components for high end/performance road cars and several motorsport customers (i.e: in F1, Le Mans etc). We use pre-preg pretty much exclusively, although I am now beginning to dabble in wet layup in my workshop at home for certain items for my own use where pre-preg would be impracticle.

Anyway, quick intro over with!

By f1rob - 1/4/2016 11:01:06 AM

Im Norfolk too but on the south coast as a composite mercenary for red bull at the moment