By 67redrocket - 12/26/2015 4:20:45 PM

What bagging is the best for infusing? Iam not using autovclave or oven for curing?

I used the VB120-EF Elastifilm Vacuum Bagging Film today and got a sealed bag cuite easy. But during infusion I started to get problems. Not shure what happend but I started to get leaks. And the leaks was located near the epoxy inlet hose. 
By Fasta - 12/28/2015 12:56:39 AM

I use Capran 518, seems great.