Talk Composites - The Forum for Advanced Composites

Degassing infusion resin, necessary?

http://www.talkcomposites.com/Topic20065.aspx

By 67redrocket - 12/22/2015 8:04:30 PM

Is it necessary to degass the resin before starting the infusion?
By 20_rc51_00 - 12/23/2015 8:08:17 PM

if you have problems with bridging you willl have huge voids. The bridging needs to be addressed. If there are very tight radi and still possibly bridging despite best efforts then degassing benefits you in reducing the chance of voids in these areas too.